CARE
Our roto-moulded kayaks are made of high-
density Super EXL linear polyethylene, which is
virtually maintenance free. A minimal amount
of care in storage and transporting will help the
kayak maintain a like-new condition for many
years.
WHITEWATER CARE
Whitewater kayaks are built to withstand
more aggressive use than recreation or touring
models. However, a certain amount of impact
and abrasion damage is to be expected
due to the nature of whitewater paddling.
Continual exposure to abrasion can roughen
the hull surface. Scratching is often cosmetic or
superficial and requires no repair.
It is important to be able to determine when
damage is cosmetic or extends to impacting
the structure of the hull. Impacts are much
more likely than scratches to result in structural
damage. Inspect your hull after suffering a collision.
As strong and durable as it is, polyethylene is
not indestructible. However, should the worst
happen, it is repairable – simply contact your
local Dagger dealer.
14
CLEANING
Usually, a quick rinse of fresh water is all that
is necessary to keep your kayak clean as well
as functioning in good order. This is very
important after paddling in salt water, particularly
if your kayak is outfitted with a rudder system.
Be sure to rinse the rudder, cables, and foot-
braces with fresh water to remove salt residue.
REPAIR OPTIONS
Although it is unlikely that your Dagger kayak
will need any repairs during its lifetime, it is
possible that a hull crack or puncture may occur
due to extreme impact or contact with a sharp
object. If this happens, first contact Dagger Europe
or your local Dagger dealer to determine if the
damage falls under the boat's warranty (see
warranty section).
We will need the serial number of your kayak,
a good description of the damage (a photo-
graph is required) and a description of the
incident during which the damage occurred.
A warranty return form is available on our web
site www.daggereurope.com.
All of this information will help us determine
the best course of action.
HULL DISTORTION
Polyethylene will become more flexible when
in warm conditions such as a hot, sunny day.
Improper storage or transportation of a plastic
boat, especially in the heat, can potentially distort
the shape of the hull on your boat.
If your kayak does become the victim of slight
distortion, correction is a simple process.
Brief exposure to the heat of the sun is often
all it takes to restore the hull to its original
shape. If that doesn't work, the hull can usually
be restored by applying heat to the outside
of the boat with a hair dryer. Take care –
high, focused heat could cause damage.
When the hull is pliable enough, it can be
pushed back into shape by hand. A weight
can be placed inside the boat to maintain the
shape of the hull as it cools. Allow 24 hours to
ensure the process is completed.
WARNING
Avoid dragging your kayak across the
ground to prolong its life and maintain its
look and performance. Two people, using
the carrying handles, is the best way to
transport a longer kayak.