12.
Torsional Forces
IMPORTANT:
Avoid putting torsional force on 900 µm fibers
being mechanically spliced (OSE-ST-4). Torsional, or
twisting, forces can cause transmission failure at
the connection after some time. The torsional force
occurs when the splice is turned and the fiber is
twisted as it is moved from the splice area and routed
in a figure-eight layout in the splice tray. Rotate the
fiber as little as possible when installing it into the
tray (Figure 15).
Corning Optical Communications LLC • PO Box 489 • Hickory, NC 28603-0489 USA
800-743-2675 • FAX: 828-325-5060 • International: +1-828-901-5000 • www.corning.com/opcomm
Corning Optical Communications reserves the right to improve, enhance, and modify the features and specifications of Corning Optical Communications products without
prior notification. A complete listing of the trademarks of Corning Optical Communications is available at www.corning.com/opcomm/trademarks. All other trademarks are
the properties of their respective owners. Corning Optical Communications is ISO 9001 certified. © 2015, 2017 Corning Optical Communications. All rights reserved.
TPA-4954
Standard Recommended Procedure 001-285 | Issue 4 | February 2017 | Page 8 of 8
Figure 15