Hot lamination double sided 70 micron pet film on up all models
Heating on both rolls => ON
The film is threaded in the machine following the diagram not using the anticurling system.
Lower the pressure rollers and start the machine, pressure setting medium.
Once the film is wrinkle free insert the substrate carefully.
Select the appropriate temp for the film you use
Note that generally :
Thinner film = less temp / slightly higher speed eg 120/ 130°C, speed 4 or 5
Thicker film = more temp / lower speed eg 140°C, speed 1 or 2
There is no hard and fast rule, find the best setting by trial.
Attention, a too high temp will tend to burn off the ink on digital print and cause speckling!
NOTE:
• Freshly printed Xerox®/Konica® production should be left to air for several hours before trying to laminate to let
the silicone oil evaporate.
• The different kinds of print will require different kinds of adhesive on the film eg super sticky for Xerox/Konica paper.
• On wax based printers the darker colours are thicker than the lighter colours due to more wax being applied to
darken the colour. This means that you can see a difference in the film height around the contour of profile of the
colour being covered by the film.
• The edge seal of the film on thicker substrates may not wrap fully due to the thickness of the substrate.
• If you trim the film close to the substrate the adhesion and sealing will be diminished.
• As soon as you stop the production raise the rolls or flat spots will occur !
Single side lamination using bopp film of ca 25 - 30micron models 360 / 460 / 660
In this case only the upper roll holder is used and the only single side switch is enabled on the back of the machine
Feed the film through the de curler you need to use.
Thicker paper => roller de curler
Thinner paper => bar de curler
By trial you will find the right height of the de curler to get the flat output
Output curling upwards => increase the de curler height
Output curling downwards => decrease the de curling height
Speed 1 to 3 depending on the film
Pressure setting higher
Heat ca 110°C to 120°C
A too high temp will blister the digital print !
Optional film strippers in position and engaged to cut the film to width