3D Systems ProJet 4500 Post Processing Manual - Page 11

Browse online or download pdf Post Processing Manual for 3D Printers 3D Systems ProJet 4500. 3D Systems ProJet 4500 13 pages. 3d professional printer
Also for 3D Systems ProJet 4500: Quick Reference Manual (19 pages)

3D Systems ProJet 4500 Post Processing Manual
3 .
Wax contains oils that may separate over long periods of time in the liquid sates . Stir the wax if it has become stagnate . Dip
the part in the wax . Dip only long enough to cover all surfaces; this should take approximately
a .
Be careful as the oven and wax are warm . Use tongs or gloves if necessary .
b.
When melting wax it will appear opaque at first but will become translucent over time.
4 .
Remove excess wax by placing the part back in the oven . Place the part above the open wax container and let any excess
wax drip off into the container . The part will need to be oriented into two (2) or more positions to clear off the bulk of the wax .
Wrapping the part in the paper towel will speed the process .
a.
Parts with small features (cross-sections ≤4mm) must to be kept under
b .
At
50°C
it will take approximately 1 hour for the wax to completely melt off the part .
c.
Large robust parts (all cross-sections ≥ 15mm) can be subjected to temperatures up to
After dipping parts are covered in wax. Keep in oven to let excess wax drip off.
3D Systems, Inc.
Dip part in wax . Use gloves or tongs if necessary .
1 Hour
11
20 seconds
50°C
to prevent distortion .
60°C
to speed the process .
for an entire part .